Polyethylene · Ex Clean Natural Regrind

W&W HDPE Regrind — 0.10 MI Fractional Melt

High-density polyethylene, fractional melt: extra-clean natural regrind

W&W Material Supply of Belding, Michigan, offers extra-clean natural fractional-melt HDPE regrind from a single source. The source resin is rated at 0.10 g/10 min melt index (190 °C / 2.16 kg) and 0.944 g/cm³ density, and the stream offers approximately 2–3 truckloads of recurring monthly volume.

Approx. availability Approximately 2–3 truckloads per month

Recurring monthly volume from a single source. Ask about current quantity and shipping details.

Material overview

This is extra-clean, natural (uncolored) regrind of a fractional-melt HDPE from a single source. A single-source stream gives buyers a known origin month to month, rather than a mixed stream from many plants.

Published data for the source resin shows a very low melt index and a high-load melt index of 8.3 g/10 min, with slow-crack-growth (PENT) of 200 hours at 80 °C, a brittleness temperature below −100 °C and notched Izod impact of 4.0 ft-lb/in: properties associated with melt strength and toughness in extrusion. Clean natural regrind of this type is commonly considered for blending with virgin fractional-melt HDPE. Regrind properties can differ from the original resin, so buyers should qualify the material for their process.

Doug can walk you through the available data and what lot-specific information can be provided before you commit to a load.

Key characteristics

  • Extra-clean natural regrind from a single source
  • Source resin: fractional melt index, 0.10 g/10 min
  • Source resin: high-load melt index 8.3 g/10 min
  • Source resin: slow crack growth (PENT) 200 hours at 80 °C
  • Source resin: brittleness temperature below −100 °C

Source-resin reference data

What these values represent: These are published values for the source resin grade this regrind comes from. They are not test results for a specific lot, and regrind properties can differ from the original resin.

HDPE Regrind — 0.10 MI Fractional Melt: source-resin reference data
Property Source-resin value Test Method
Density — natural 0.944 g/cm³ ASTM D792
Melt Index, 190 °C / 2.16 kg 0.10 g/10 min ASTM D1238
High-Load Melt Index, 190 °C / 21.6 kg 8.3 g/10 min ASTM D1238
Tensile Strength at Yield 3,200 psi (22.1 MPa) ASTM D638
Tensile Elongation at Break 850% ASTM D638
Flexural Modulus 120,000 psi (827 MPa) ASTM D790B
Slow Crack Growth, PENT @ 80 °C 200 hr ASTM F1473
Notched Izod Impact @ 23 °C 4.0 ft-lb/in (210 J/m) ASTM D256A
Brittleness Temperature < −148 °F (< −100 °C) ASTM D746A
Thermal Stability > 482 °F (> 250 °C) ASTM D3350
Suggested Melt Temperature 380–440 °F (193–227 °C) —

Published values are reference data, labeled on each page for what they represent. Ask W&W what lot-specific test data or documentation is available for a given shipment, and confirm your requirements before purchase.

Common applications for this resin type

  • Extrusion processes requiring high melt strength
  • Non-pressure pipe, conduit and profile extrusion
  • Thick-wall and heavy-gauge extruded parts
  • Blending with virgin fractional-melt HDPE

As regrind, this material is not represented for potable-water, gas-distribution or other regulated pressure-pipe applications, and W&W does not represent it as holding any listing or certification. Ask W&W what documentation is available for a specific lot.

Ask about this material

Tell us the quantity you need, whether it is one-time or recurring, your application and your delivery location, or simply start with a question. Pricing and current availability are discussed directly. You can also call Doug at 302-588-3033 or email dworen53@gmail.com.

Ask About This Material

Other current materials

Let’s connect.

Whether you’re looking for material, have something to sell, or simply want to discuss an opportunity, we’d welcome the conversation.